Technetium, Tc; Annealed
Subcategory: Pure Element; Nonferrous Metal
Close Analogs: See also As-Rolled Tc.
Material Notes: Annealed applies only to tensile and/or hardness values; other property values are typical of the element. Property values for Tc-99. Annealed 10 min at 950°C (1740°F)
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Magnetic Susceptibility
- Critical Magnetic Field Strength, Oersted
- Critical Superconducting Temperature
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- CAS Number
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|