Alumina, 99.9%, Al2O3
Subcategory: Oxide, Aluminum; Oxide
Key Words: Alpha alumina, Al2O3, aluminum oxide, corundum, aluminium oxide
Material Notes: Property values below are taken from literature and manufacturer sources. Variations are possible among various commercial grades.
| Available Properties |
- Density
- Water Absorption
- a Lattice Constant
- c Lattice Constant
- Formula Units/Cell (Z)
- Molecular Weight
- Weibull Modulus
- Hardness, Knoop
- Hardness, Vickers
- Vickers Microhardness
- Hardness, Mohs
- Abrasive Hardness
- Drilling Hardness
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Strength
- Compressive Yield Strength
- Poissons Ratio
- Fracture Toughness
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- Magnetic Susceptibility
- Dielectric Constant
- Dielectric Strength
- Heat of Fusion
- CTE, linear 250°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Boiling Point
- Maximum Service Temperature, Air
- Refractive Index
- Color
- Crystal Structure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|