Alumina, 99.9%, Al2O3

 

Subcategory: Oxide, Aluminum; Oxide

Key Words: Alpha alumina, Al2O3, aluminum oxide, corundum, aluminium oxide

Material Notes:
Property values below are taken from literature and manufacturer sources. Variations are possible among various commercial grades.

Available Properties
  • Density
  • Water Absorption
  • a Lattice Constant
  • c Lattice Constant
  • Formula Units/Cell (Z)
  • Molecular Weight
  • Weibull Modulus
  • Hardness, Knoop
  • Hardness, Vickers
  • Vickers Microhardness
  • Hardness, Mohs
  • Abrasive Hardness
  • Drilling Hardness
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • Flexural Strength
  • Compressive Yield Strength
  • Poissons Ratio
  • Fracture Toughness
  • Shear Modulus
  • Electrical Resistivity
  • Electrical Resistivity at Elevated Temperature
  • Magnetic Susceptibility
  • Dielectric Constant
  • Dielectric Strength
  • Heat of Fusion
  • CTE, linear 250°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Boiling Point
  • Maximum Service Temperature, Air
  • Refractive Index
  • Color
  • Crystal Structure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。