Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Subcategory: Oxide, Other; Oxide; Ceramic
Key Words: Ca10(PO4)6(OH)2
Material Notes: Calcium hydroxyapatite is a natural constituent of teeth and bone, along with other calcium-phosphate ceramic (CPC) materials. Synthetic hydroxyapatite is used as an active bioceramic for teeth and bone replacement. Ionic substitution is common and plays a large role in the structure and properties of hydroxyapatites.
| Available Properties |
- Density
- Porosity
- a Lattice Constant
- c Lattice Constant
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
- Poissons Ratio
- Unit Cell
|
|
|
|