Pyrolytic Graphite, Low Temperature Isotropic (LTI)
Subcategory: Graphite; Carbon
Material Notes: LTI carbon is deposited from a fluidized bed (from pyrolyzed hydrocarbons) onto a substrate at temperatures below 1500°C. The properties, including density, vary depending on the deposition conditions.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Strength
- Compressive Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|