Albite (Feldspar NaAlSi3O8)
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Key Words: Albite (Feldspar NaAlSi3O8)
Material Notes: Two cleavage directions. Weathering end products: Kaolinite, illite. Occurrence: Igneous and metamorphic rocks. All feldspars are good indicators of the rock freshness. Property values are typical of naturally occurring Albite (Feldspar NaAlSi3O8). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Hardness, Mohs
- CTE, linear 20°C
- CTE, linear 500°C
- Color
|
|
|
|
| Property Data |