Andesite
Material Notes: Igneous rock, with a fine texture and grain size < 1mm (extrusive). It is intermediate in the acidic-basic range, with a total silica content of 55-65%. Predominent minerals in this generally medium-dark colored rock are horneblende and plagioclase feldspar. Property values are typical of naturally occurring Andesite (Felsite). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Porosity
- Modulus of Elasticity
- Specific Heat Capacity
|
|
|
|