Augite (Iron-Magnesium Silicate)
Subcategory: Oxide, Silicon; Oxide
Material Notes: Two cleavage directions. Weathering end products: Brown clay, limonite. Occurrence: Igneous, metamorphic. Property values are typical of naturally occurring Augite (Iron-Magnesium Silicate). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Hardness, Mohs
- CTE, linear 20°C
- CTE, linear 500°C
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|