Bischofite (MgCl2-6H2O)
Subcategory: Halide
Key Words: Bischofite (MgCl2-6H2O)
Material Notes: Critical relative humidity for stability is 33%. Crystallization Pressure for C/CS = 2 is 119 atm at 0°C. Crystallization Pressure for C/CS = 2 is 142 atm at 50°C. Crystallization Pressure for C/CS = 10 is 397 atm at 0°C. Crystallization Pressure for C/CS = 10 is 470 atm at 50°C.Crystallization Pressure for C/CS = 50 is 675 atm at 0°C. Crystallization Pressure for C/CS = 50 is 803 atm at 50°C. Property values are typical of naturally occurring Bischofite (MgCl2-6H2O). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Solubility
- Molecular Weight
- Molar Volume
|
|
|
|