|   Dodekahydrate (MgSO4-12H2O)  Key Words: Dodekahydrate (MgSO4-12H2O) Material Notes: Crystallization Pressure for C/CS = 2 is 67 atm at 0°C.  Crystallization Pressure for C/CS = 2 is 80 atm at 50°C.Crystallization Pressure for C/CS = 10 is 222 atm at 0°C.  Crystallization Pressure for C/CS = 10 is 264 atm at 50°C.Crystallization Pressure for C/CS = 50 is 378 atm at 0°C.  Crystallization Pressure for C/CS = 50 is 450 atm at 50°C.
 Property values are typical of naturally occurring  Dodekahydrate (MgSO4-12H2O).  Actual property values will vary from sample to sample. 
| | 
    | Available Properties |  
    | DensityMolecular WeightMolar Volume
 | 
 | 
 |  | | 