Dodekahydrate (MgSO4-12H2O)
Key Words: Dodekahydrate (MgSO4-12H2O)
Material Notes: Crystallization Pressure for C/CS = 2 is 67 atm at 0°C. Crystallization Pressure for C/CS = 2 is 80 atm at 50°C.Crystallization Pressure for C/CS = 10 is 222 atm at 0°C. Crystallization Pressure for C/CS = 10 is 264 atm at 50°C.Crystallization Pressure for C/CS = 50 is 378 atm at 0°C. Crystallization Pressure for C/CS = 50 is 450 atm at 50°C. Property values are typical of naturally occurring Dodekahydrate (MgSO4-12H2O). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Molecular Weight
- Molar Volume
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|