Dolomite (Ca,Mg)(CO3)2
Key Words: Dolomite (Ca,Mg)(CO3)2
Material Notes: Weathering end products: Limestones, dolomites, marbles. Occurrence: Dolomites, marbles. Property values are typical of naturally occurring Dolomite (Ca,Mg)(CO3)2. Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Porosity
- Solubility
- Hardness, Mohs
- Modulus of Elasticity
- CTE, linear 20°C
- Thermal Conductivity
- Color
|
|
|
|