Glauconite (K, Ca, Na),(Al, Fe", Fe"',Mg)2({OH}2Si3AlO10)
Key Words: Glauconite (K, Ca, Na),(Al, Fe'', Fe''',Mg)2({OH}2Si3AlO10)
Material Notes: One cleavage direction. Occurrence: Sediments. Important green pigment. Property values are typical of naturally occurring Glauconite (K, Ca, Na),(Al, Fe'', Fe''',Mg)2({OH}2Si3AlO10). Actual property values will vary from sample to sample.
|
|
|
| Property Data |