Labradorite (Feldspar; 60% CaAl2Si2O8 + 40% NaAlSi3O8)
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Key Words: Labradorite (Feldspar; 60% CaAl2Si2O8 + 40% NaAlSi3O8)
Material Notes: Two cleavage directions. Weathering end product(s): Kaolinite illite. Occurrence: Igneous rocks metamorphic. All feldspars are good indicators of the rock freshness. Property values are typical of naturally occurring Labradorite (Feldspar; 60% CaAl2Si2O8 + 40% NaAlSi3O8). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Hardness, Mohs
- CTE, linear 20°C
- CTE, linear 500°C
- Color
|
|
|
|
| Property Data |