Marcasite (FeS2)
Subcategory: Sulfide/Chalcogenide
Key Words: Marcasite (FeS2)
Material Notes: Weathering end product: Limonite. Occurrence: Sediments. SO2 ion released during weathering, which may oxidize to SO3. Property values are typical of naturally occurring Marcasite (FeS2). Actual property values will vary from sample to sample.