Mirabilite (Na2SO4)-10H2O)
Key Words: Mirabilite (Na2SO4)-10H2O)
Material Notes: Critical relative humidity for stability is 94%. Crystallization Pressure for C/CS = 2 is 72 atm at 0°C. Crystallization Pressure for C/CS = 2 is 83 atm at 50°C. Crystallization Pressure for C/CS = 10 is 234 atm at 0°C. Crystallization Pressure for C/CS = 10 is 277 atm at 50°C.Crystallization Pressure for C/CS = 50 is 397 atm at 0°C. Crystallization Pressure for C/CS = 50 is 473 atm at 50°C. Property values are typical of naturally occurring Mirabilite (Na2SO4)-10H2O). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Molecular Weight
- Molar Volume
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|