Montmorillonite Al2O3-4SiO2-nH2O
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Key Words: Montmorillonite Al2O3-4SiO2-nH2O
Material Notes: One cleavage direction. End product from the weathering of stone used for construction. Occurrence: Sediments. Swelling clay; Swelling pressure to 9000 psi. Property values are typical of naturally occurring Montmorillonite Al2O3-4SiO2-nH2O. Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Hardness, Mohs
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|