Muscovite (KAl2(AlSi3O10)-(OH)2)
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Key Words: Muscovite (KAl2(AlSi3O10)-(OH)2)
Material Notes: One cleavage direction. Occurrence: Igneous, sediments, metamorphic. Very resistant to weathering. Property values are typical of naturally occurring Muscovite (KAl2(AlSi3O10)-(OH)2). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Hardness, Mohs
- Color
|
|
|
|
| Property Data |