Tachhydrite (2MgCl2-CaCl2-12H2O)
Subcategory: Halide
Key Words: Tachhydrite (2MgCl2-CaCl2-12H2O)
Material Notes: Crystallization Pressure for C/CS = 2 is 50 atm at 0°C. Crystallization Pressure for C/CS = 2 is 59 atm at 50°C. Crystallization Pressure for C/CS = 10 is 166 atm at 0°C. Crystallization Pressure for C/CS = 10 is 198 atm at 50°C.Crystallization Pressure for C/CS = 50 is 282 atm at 0°C. Crystallization Pressure for C/CS = 50 is 336 atm at 50°C. Property values are typical of naturally occurring Tachhydrite (2MgCl2-CaCl2-12H2O). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- Molecular Weight
- Molar Volume
|
|
|
|
| Property Data |