Thenardite (Na2SO4)
Key Words: Thenardite (Na2SO4)
Material Notes: Critical relative humidity for stability is 82%. Crystallization Pressure for C/CS = 2 is 292 atm at 0°C. Crystallization Pressure for C/CS = 2 is 345 atm at 50°C. Crystallization Pressure for C/CS = 10 is 970 atm at 0°C. Crystallization Pressure for C/CS = 10 is 1150 atm at 50°C.Crystallization Pressure for C/CS = 50 is 1650 atm at 0°C. Crystallization Pressure for C/CS = 50 is 1965 atm at 50°C. Property values are typical of naturally occurring Thenardite (Na2SO4). Actual property values will vary from sample to sample.