Thermonatrite (Na2CO3 - H2O)
Key Words: Thermonatrite (Na2CO3 - H2O)
Material Notes: One cleavage direction. Occurrence: Desert floor stone pores. Important in salt bursting. Crystallization Pressure for C/CS = 2 is 280 atm at 0°C. Crystallization Pressure for C/CS = 2 is 333 atm at 50°C. Crystallization Pressure for C/CS = 10 is 935 atm at 0°C. Crystallization Pressure for C/CS = 10 is 1109 atm at 50°C.Crystallization Pressure for C/CS = 50 is 1590 atm at 0°C. Crystallization Pressure for C/CS = 50 is 1891 atm at 50°C. Property values are typical of naturally occurring Thermonatrite (Na2CO3 - H2O). Actual property values will vary from sample to sample.