Mica (K(Mg,Fe)3(AlSi3O10)(OH)2)
Subcategory: Oxide, Silicon; Oxide
Key Words: K(Mg,Fe)3(AlSi3O10)(OH)2
Material Notes: Silicates of alumina with hydrogen (hydrous alumino silicates) iron and magnesia (Biotite)
| Available Properties |
- Specific Gravity
- Hardness, Mohs
- Cleavage
- Color
- Durability
- Luster
- Streak
|
|
|
|