Fused Quartz
Subcategory: Oxide, Silicon; Oxide
Key Words: SiO2
Material Notes: Silicon dioxide. Information below is typical for commercially available fused quartz used for tubing and lighting applications. A wide variation of properties is possible between specific grades.
Available Properties |
- Density
- Water Absorption
- Hardness, Knoop
- Hardness, Mohs
- Modulus of Elasticity
- Compressive Yield Strength
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Dielectric Constant
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Softening Point
- Annealing Point
- Strain Point
- Refractive Index
- Transmission, Visible
- Color
|
|
|
|
Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|