Silver Vanadium Oxide Fluoride, Ag4V2O6F2
Subcategory: Oxide, Other; Halide; Oxide
Key Words: SVOF, primary lithium battery cathode
Material Notes: Silver Vanadium Oxide Fluoride, Ag4V2O6F2 (SVOF) is a being researched as a cathode for for high capacity lithium batteries. It has a higher accessible silver content and a higher capacity than the commercial cathode material Silver Vanadium Oxide (SVO; Ag2V4O11). The SVOF cathode maintains a greater potential than SVO electrodes for extended periods of time, allowing optimal device performance essential for medical battery applications, such as implantable defibrillators. When used as a cathode in a lithium battery, SVOF has two distinct regions within the discharge curve - an upper plateau at 3.5 V attributed to silver reduction and a lower sloped region around 2.3 V attributed to the reduction of the vanadium oxide fluoride framework.
| Available Properties |
- Density
- a Lattice Constant
- b Lattice Constant
- c Lattice Constant
- Beta Lattice Angle
- Formula Units/Cell (Z)
- Molecular Weight
- Capacity (Battery)
- Space Group
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|