AO 98 Aluminum Oxide Ceramic Substrate, 98% Purity
Subcategory: Oxide, Aluminum; Oxide
Key Words: Alumina; Al2O3; Corundum; MarkeTech International; Ceramics
Material Notes: Data provided by the supplier, MarkeTech International. Substrate Specs: Maximum dimensions 4.0 x 6.0 in.. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µm polished.
| Available Properties |
- Density
- Flexural Strength
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|