GE Advanced Ceramics AC6091 Boron Nitride (BN) Powder

 

Subcategory: Nitride; Additive/Filler for Polymer

Material Notes:
GE Advanced Ceramics boron nitride (BN) powder grades AC6028, AC6103, and AC6091 are large agglomerates of well-defined individual (~10 µm) crystals. These low- to medium-density grades are processed to achieve tailored surface areas; they are pourable and exhibit good lubrication and thermal conductivity properties in finished products.

AC6091 is similar in particle size to AC6028 (average particle size of 125 µm), but is refined to achieve a lower surface area and higher tap density.

Applications: These grades are ideal for use in thermal spray applications as well as metal-matrix and ceramic composites for wear applications such as high-performance brake linings. They are also used in heating elements and adhesives, pastes, and potting compounds with increased thermal conductivity and high electrical resistivity.

Information provided by GE Advanced Ceramics.

Available Properties
  • Density
  • Particle Size
  • Specific Surface Area
  • Carbon
  • Color
  • Crystal Type
  • Oxygen
  • Sol. Borate
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。