GE Advanced Ceramics HCM Boron Nitride (BN) Powder
Subcategory: Nitride; Additive/Filler for Polymer
Material Notes: GE Advanced Ceramics boron nitride (BN) powder grades HCR48, HCJ48, and HCM are large, high-density agglomerates, of ~10 µm crystals, with average particle sizes between 175-275 µm and tap densities of ~1 g/cm3. These features, combined with low average surface areas, give powders that flow readily, withstand harsh processing, and have outstanding thermal characteristics. HCM has a slightly finer average particle size of 175 µm and is processed for outstanding purity, making it appropriate for the most demanding of applications. HCM also has a more uniform particle size distribution and rounded particles due to its unique processing. Information provided by GE Advanced Ceramics.
| Available Properties |
- Density
- Particle Size
- Specific Surface Area
- Carbon
- Color
- Crystal Type
- Oxygen
- Sol. Borate
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|