GE Advanced Ceramics AC-6028 Boron Nitride (BN) Powder
Subcategory: Nitride
Material Notes: Grade AC-6028 consists of agglomerated particles of hexagonal Boron Nitride (BN) with a mean particle size between 100 and 150µ. It exhibits the unique properties of BN in a form readily used in many advanced materials and processes. Grade AC-6028 is processed to achieve relatively large crystals and low surface area which contribute to excellent thermal properties and flow characteristics. Boron Nitride powders are produced by GE Advanced Ceramics in more than 50 individual (standard and custom) grades to meet a wide variety of application needs. For use in: Electrically insulating/thermally conductive fillers for heaters, polymer matrices, adhesives, pastes and potting compounds. Lubrication applications for extreme heat or cold, extreme pressure, vacuum environments or harsh chemical exposures. Refractories and refractory coatings. Mold/die release. Metal/ceramic and ceramic/matrix composites. General Characteristics of Boron Nitride: Electrical Insulator, Low Dielectric Constant, Low Dielectric Loss, High Temperature Stability, Thermal Conductor, Lubricious, Inert, Non-Wetting. Information provided by GE Advanced Ceramics.
| Available Properties |
- Apparent Bulk Density
- Particle Size
- Specific Surface Area
- Color
- Crystal Structure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|