GE Advanced Ceramics Pyrolytic Boron Nitride (PBN) Coating
Subcategory: Nitride; Ceramic/Metallic Coating
Material Notes: High temperature protective coating for graphite. PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite from very corrosive atmospheres including most molten metals, all acids, and hot ammonia. PBN is an electrical insulator which exhibits a high degree of anisotropy, e.g. good thermal conductor parallel ("ab") to substrate and thermal insulator through thickness ("c"). Information provided by GE Advanced Ceramics.
| Available Properties |
- Density
- Modulus of Elasticity
- Compressive Yield Strength
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Emissivity (0-1)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|