GE Advanced Ceramics HOPG Graphite Monochromator
Subcategory: Graphite; Carbon
Material Notes: Advanced Ceramics' graphite monochromators are highly oriented forms of high purity pyrolytic graphite which diffract x-rays and neutrons with greater efficiency than any other material. In x-ray analysis, intensity is increased 3 to 5 times over that obtained with conventionally used crystals. A singly-bent focusing monochromator using graphite yields 3 times the intensity of lithium fluoride at equivalent resolution. GE Advanced Ceramics originally introduced, and still offers, graphite monochromators with the lowest mosaic spread (>= 0.4°) available. Information provided by GE Advanced Ceramics.
| Available Properties |
- Density
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|