GE Advanced Ceramics PolarTherm® PT131 Boron Nitride (BN) Powder

 

Subcategory: Nitride; Additive/Filler for Polymer

Material Notes:
Boron Nitride powders are produced by GE Advanced Ceramics in more than 50 individual (standard and custom) grades to meet a wide variety of application needs.

For use in:

  • Electrically insulating/thermally conductive fillers for heaters, polymer matrices, adhesives, pastes and potting compounds.
  • Lubrication applications for extreme heat or cold, extreme pressure, vacuum environments or harsh chemical exposures.
  • Refractories and refractory coatings.
  • Mold/die release.
  • Metal/ceramic and ceramic/matrix composites.

General Characteristics of Boron Nitride:

  • Electrical Insulator
  • Low Dielectric Constant
  • Low Dielectric Loss
  • High Temperature Stability
  • Thermal Conductor
  • Lubricious
  • Inert
  • Non-Wetting

PT131 has been processed for higher purity than PT130 and has a slightly larger mean particle size (10 µm) and higher surface area.

Information provided by GE Advanced Ceramics.

Available Properties
  • Density
  • Particle Size
  • Specific Surface Area
  • Calcium
  • Carbon
  • Color
  • Crystal Type
  • Oxygen
  • Sol. Borate
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。