Advanced Ceramics Limited Zinc Alumino-Silicate ACL 2088
Subcategory: Glass Ceramic; Oxide, Aluminum; Oxide
Material Notes: A low expansion glass-ceramic suitable for sealing to molybdenum.Information provided by Advanced Ceramics Limited (ACL)
| Available Properties |
- Density
- Modulus of Elasticity
- Modulus of Rupture
- Volume Resistivity
- Dielectric Strength
- CTE, linear 500°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|