Advanced Ceramics Limited Lithium Alumino-Silicate ACL 2087
Subcategory: Oxide, Silicon; Glass Ceramic; Oxide
Material Notes: A high strength glass-ceramic suitable for sealing to 17% chrome-iron or Nilo 48Information provided by Advanced Ceramics Limited (ACL)
| Available Properties |
- Density
- Hardness, Rockwell HR45N
- Modulus of Elasticity
- Modulus of Rupture
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 100°C
- CTE, linear 1000°C
|
|
|
|