Anderman Ceramics EZC96 Zirconia, 96%, Calcia-Stabilized
Subcategory: Oxide, Zirconium; Oxide
Key Words: ZrO2
Material Notes: Available in impervious or porous grades in a range of shapes and sizes. Information provided by Anderman Ceramics.
| Available Properties |
- Density
- Open Porosity
- Maximum Service Temperature, Air
- Thermal Shock Resistance
|
|
|
|