AREMCO Cerama-bond™ 3062
Subcategory: Oxide, Silicon; Oxide
Close Analogs: This grade is no longer in AREMCOs product line
Material Notes: Chemical setting. Single-part ceramic for glass-to-metal areas up to 1" diam. x 3/4" deep. Used to pot small temperature sensors, gas igniters, and high intensity lights. Applied in areas up to 1" diameter by 1" depth, then air set for 2-4 hours and cured at 200 ºF prior to operation. Two-part systems are used to produce high temperature molds and fixtures. Data provided by the manufacturer, AREMCO Products, Inc. AREMCO Products, Inc. makes no warranty express or implied concerning the use of these products. The user assumes all risk of use or handling whether or not in accordance with directions or suggestions, or used singly or in combination with other products.
| Available Properties |
- Open Porosity
- Compressive Yield Strength
- Electrical Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|