AREMCO AREMCOLOX™ Machinable and Fired Ceramics 502-1550 (Low Density) Zirconium Phosphate
Subcategory: Oxide, Other; Machinable Ceramic; Oxide
Material Notes: Ultra high thermal shock resistance and low thermal conductivity. For brazing fixtures, induction heating liners, rocket nozzles and high temp gauges, tooling and structures. Plates from 1/4" to 1" thick; rods from 1/2" to 2" diameter.Information provided by AREMCO
| Available Properties |
- Specific Gravity
- Density
- Porosity
- Hardness, Mohs
- Flexural Strength
- Compressive Strength
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 68°F
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|