AREMCO AREMCOLOX™ Machinable and Fired Ceramics 502-1600 (99%) Boron Nitride 99%
Subcategory: Nitride; Machinable Ceramic
Material Notes: Hot-pressed high purity 99% boron nitride. High thermal conductivity. Easily machined. Non-reactive in molten salts, aluminum and other metals. Plates from 1/4" to 1" thick; rods from 1/4" to 3" diameter; bars from 1/4" x 1/4" to 2"x 2".Information provided by AREMCO
| Available Properties |
- Specific Gravity
- Density
- Porosity
- Flexural Strength
- Compressive Strength
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 68°F
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |