AREMCO AREMCOLOX™ Machinable and Fired Ceramics 502-1800 Aluminum Nitride
Subcategory: Nitride; Machinable Ceramic
Material Notes: Hot-pressed Aluminum nitride. Ultra high thermal conductivity and dielectric strength. Readily machined. Plates from 1/4" to 1" thick, custom rod available upon request.Information provided by AREMCO
| Available Properties |
- Specific Gravity
- Density
- Porosity
- Hardness, Mohs
- Compressive Strength
- Dielectric Constant
- Dielectric Strength
- CTE, linear 68°F
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |