AREMCO Pyro-Putty™ 2500 High Temperature Ceramic-Metallic Putties, Iron Oxide Filled
Subcategory: High Temp Ceramic Resin; Ceramic
Material Notes: Ceramic and Black Iron Oxide-Filled, One-Part, Water Based Paste. For Applications to 1/4" Thick. Repairs Cast Iron, and Steel Parts to 1600°FInformation provided by AREMCO