AREMCO Ceramacast High Temperature Potting & Casting Material 584 Magnesia
Subcategory: Oxide, Magnesium; Oxide
Material Notes: Two-part, quick-set ceramic for small parts.Information provided by AREMCO
| Available Properties |
- Density
- Porosity
- Viscosity
- Compressive Strength
- Volume Resistivity
- Dielectric Strength
- CTE, linear 68°F
- Maximum Service Temperature, Air
- Shrinkage
- Dry Time
- Cure Time
- Pot Life
- Shelf Life
- Acid Resistance
- Alkali Resistance
|
|
|
|