AREMCO Corr-Paint™ High Temperature Protective Coating CP3015 Inorganic, Mixed Oxides Filled
Subcategory: Ceramic/Metallic Coating
Material Notes: For exceptional corrosion and temperature resistance to 1400ºF. Available in standard metallic grey as well as aluminum CP3015-AL, and black CP3015-BL formulations. This advanced material is specially formulated to adhere to steel and refractory products used in boilers, furnaces, kilns, stacks, and other high temperature structures. Benefits include extended equipment life, lower energy costs, and increased throughput.Information provided by AREMCO
| Available Properties |
- Specific Gravity
- Solids Content
- Volatile Organic Compounds (VOC) Content
- Viscosity
- Thickness
- Storage Temperature
- Maximum Service Temperature, Air
- Processing Temperature
- Dry Time
- Cure Time
- Shelf Life
- Dry Film Coverage ft2/gal
- Thinner
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|