AREMCO Cerama-Bind™ 642 High Temperature Inorganic Binders
Subcategory: Adhesive
Material Notes: A basic solution which is highly compatible with most ceramic and metal powders. Good wettability and tack, and excellent acid resistance after curing. Extremely moisture resistant after a high temperature cure. Sets up in thick cross-sections when properly formulated.Information provided by AREMCO
| Available Properties |
- Specific Gravity
- Solids Content
- pH
- Viscosity
- Storage Temperature
- Maximum Service Temperature, Air
- Shelf Life
|
|
|
|
| Property Data |