AREMCO Cerama-Bind™ 644-S High Temperature Inorganic Binders
Subcategory: Adhesive
Material Notes: A colloidal silica aqueous solution which produces high adhesive strength. Ideal for blending with all types of granular and fibrous ceramics. Excellent resistance to temperature, moisture and mechanical shock.Information provided by AREMCO
| Available Properties |
- Specific Gravity
- Solids Content
- pH
- Viscosity
- Storage Temperature
- Maximum Service Temperature, Air
- Shelf Life
|
|
|
|