AREMCO Cerama-Bind™ 875 High Temperature Inorganic Binders
Subcategory: Adhesive
Material Notes: An acidic powdered binder system used to formulate high strength, hydraulic-setting cements for electrical potting or molding applications. A powder blend is typically formulated by adding one part binder to four parts filler by weight. Water is then added in a ratio of 15-20 parts to 100 parts powder blend by weight. Curing occurs at room temperature or can be accelerated by heating at 200 °F for 1-2 hours.Information provided by AREMCO
| Available Properties |
- Specific Gravity
- Solids Content
- pH
- Storage Temperature
- Maximum Service Temperature, Air
- Cure Time
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|