ATI Wah Chang Hafnium Tetrachloride LZ (Low Zirconium) Grade, HfCl4
Subcategory: Polyester, TS
Close Analogs: Typical Analysis: On Hf metal basis
Material Notes: A white anhydrous powder.Information provided by ATI Wah Chang
| Available Properties |
- Bulk Density
- Molecular Weight
- Nominal Purity %
|
|
|
|