BACT DLC Diamond-Like Coating
Subcategory: Diamond; Carbon; Ceramic/Metallic Coating
Material Notes: DLC (a-C:H). This coating provides the highest hardness and abrasion resistance of the BACT products. Typical applications include high wear environments involving seals, molds, metal forming, and powder compaction. Applied using a PACVD (plasma-assisted physical vapor deposition) coating method. Diamond-like coatings are amorphous carbon-based coatings that exhibit high hardness and low coefficients of friction. Their unique composition and structure result in excellent wear resistance and non-stick characteristics. These coatings are thin, chemically inert, corrosion resistant, have minimal particulate contamination, tailorable electrical resistivities, and have a very low surface roughness. Information provided by Bekaert Advanced Coating Technologies (BACT).
| Available Properties |
- Thickness
- Hardness, Rockwell C
- Coefficient of Friction
- K (wear) Factor
- Electrical Resistivity
- Dielectric Strength
- Maximum Service Temperature, Air
- Processing Temperature
- Microhardness
- Surface Energy
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|