CeramTec Grade 698 Pink 96% Alumina (Al2O3)
Subcategory: Oxide, Aluminum; Oxide
Key Words: Al2O3; Aluminum Oxide
Material Notes: Te value is 840°C. Hasselman Thermal Shock value is 200 K. Data provided by CeramTec North America.
| Available Properties |
- Density
- Water Absorption
- Vickers Microhardness
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Strength
- Compressive Yield Strength
- Poissons Ratio
- Fracture Toughness
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Dielectric Loss Index
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|