CeramTec Grade 193 Gray Titania (TiO2)
Subcategory: Oxide, Titanium; Oxide
Key Words: TiO2; Titanium Dioxide
Material Notes: Te value is 520°C. Hasselman Thermal Shock value is 330 K. Data provided by CeramTec North America.
| Available Properties |
- Density
- Water Absorption
- Vickers Microhardness
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Strength
- Compressive Yield Strength
- Poissons Ratio
- Fracture Toughness
- Shear Modulus
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|