Ceradyne Ceralloy® BeO
Subcategory: Oxide, Other; Oxide
Material Notes:
Applications: collector rodshelix supportswindowsFeatures: higher thermal conductivity at room temperature. Information provided by Ceradyne Company
| Available Properties |
- Flexural Strength
- Dielectric Constant
- CTE, linear 1000°C
- Thermal Conductivity
- Composition
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|