Ceradyne Ceralloy® 398J Yttrium Oxide
Subcategory: Oxide, Other; Oxide
Material Notes: Ceralloy® 398J Hot Pressed Yttrium Oxide is a high purity hot-pressed ceramic exhibiting excellent corrosion and erosion resistance. Products produced from Hot Pressed Yttrium Oxide are for semiconductor wafer processing applicationsInformation provided by Ceradyne Company
| Available Properties |
- Density
- Vickers Microhardness
- Modulus of Elasticity
- Flexural Strength
- Poissons Ratio
- Fracture Toughness
- Electrical Resistivity
- CTE, linear 1000°C
- Thermal Conductivity
- Purity, %
|
|
|
|